# Radiating crack (ISO 6520-1 ref. 103): causes and detection

Source: https://www.therness.com/defects/103-radiating-crack/
Language: en

ISO 6520-1 group 1 · Cracks

ISO 6520-1 reference 103 is a set of cracks radiating outward from one shared origin point, typically a hard or embrittled spot. Cause matrix, the rule that tells it apart from a branching crack, and where acceptance is set.

ISO 6520-1 reference

103

Group

1 — Cracks

Also called

Radiating crack, Star cracking, Radial cracking

Full guide

[Radiating crack: the long-form guide](https://www.therness.com/blog/weld-cracks-hot-cold-types-causes-prevention/)

This page is the reference card — causes, detection and where acceptance is defined. The guide covers the subject in depth.

A radiating crack is several cracks, not one, all starting from a single shared point rather than running independently through the weld or parent metal. ISO 6520-1 reference 103 names that shared-origin pattern, distinguishing it from a single crack that later splits — [branching crack](https://www.therness.com/defects/106-branching-crack/), 106 — and from several unconnected cracks scattered through the same region — [group of disconnected cracks](https://www.therness.com/defects/105-group-of-disconnected-cracks/), 105.

The shared point can be several things: a local hard zone from an arc strike or grinding burn, a crater or restart where shrinkage strain concentrates, or a buried inclusion or lack-of-fusion pocket a crack nucleates against. Each is a single small-volume stress concentration that a crack can radiate outward from once hydrogen or service stress reaches it.

The practical lesson is where to put inspection effort: every incidental heating mark, crater, restart, and buried NDT indication the fabrication picked up — not only the planned line of the joint — is a candidate origin.

## Typical causes

What produces radiating crack, the mechanism, and the control that removes it

| Cause | Mechanism | Control |
| --- | --- | --- |
| An accidental arc strike outside the joint | Rapid local melting followed by a fast quench against cold parent metal leaves a small, hard zone under the strike. | Treat every arc strike as a finding to evaluate, never grind and repaint without inspection. |
| A crater or a stop/start point on the same weld | The last liquid metal to solidify, at a crater or a restart, concentrates shrinkage strain into one small volume, and cracks can radiate outward from it. | Grind out and re-fill every crater and restart before final inspection; never leave one as the last event on the joint. |
| An existing subsurface imperfection acting as a stress-raiser | A slag inclusion or lack-of-fusion pocket buried in an otherwise sound weld is a sharp discontinuity; stress concentrates there, and a crack can nucleate at it and radiate outward through the weld or HAZ metal. | Treat any NDT indication of a buried inclusion or lack-of-fusion as a location to re-examine for radiating cracking, not only as its own defect. |

## Detection: which route finds it

The column that matters most is the last one. An inspection family marked as not finding this imperfection will not find it however carefully it is applied, and planning around that is cheaper than discovering it during a final examination.

Detection routes for radiating crack, and what each one can and cannot see

| Family | Method | Capability | What it sees |
| --- | --- | --- | --- |
| Visual | Visual testing to ISO 17637 | Supporting signal | An arc strike or grinding burn is visible before it cracks; catching the mark itself is worth more than finding the crack later. |
| Thermal | In-process infrared thermography | Supporting signal | Flags planned heating in the joint; an accidental strike away from it is only caught if the field of view happens to include it. |
| Camera | High-speed weld pool imaging | Does not find it | Watches the weld pool itself; an accidental strike elsewhere, and the crack that later radiates from it, sit outside that view. |
| NDT | Magnetic particle or penetrant testing to ISO 17638 and ISO 3452-1, ultrasonic for depth | Primary route | Surface testing finds the radiating pattern; ultrasonic sizes how deep the hard zone runs under the strike. |

## Where acceptance is defined

Therness pages never reproduce a standard's acceptance values: those tables are copyrighted and belong in the copy you hold. What follows is the pointer — which document governs, and which part of it to open.

Documents that set the acceptance criteria, and the clause topic to read

| Standard | Clause topic | Note |
| --- | --- | --- |
| ISO 5817 | Quality levels for imperfections indexed by ISO 6520-1 reference number; every crack, radiating cracks included, is excluded from every level | A radiating crack gets no different treatment than any other crack: excluded, not graded down. |
| AWS D1.1 | Structural welding acceptance, treating an arc strike as its own finding before any crack from it is assessed | The strike is checked and disposed of on its own terms first. |

## Standards that govern this imperfection

- [ISO 5817](https://www.therness.com/standards/iso-5817/)Does ISO 5817 govern your joint? Scope decision flow for the steel, nickel and titanium quality-level standard, the codes it is read with, and the records that evidence conformity.

## Imperfections found alongside it

- [Branching crack (ref. 106)](https://www.therness.com/defects/106-branching-crack/)Cracks — ISO 6520-1 group 1.
- [Group of disconnected cracks (ref. 105)](https://www.therness.com/defects/105-group-of-disconnected-cracks/)Cracks — ISO 6520-1 group 1.
- [Arc strike (ref. 601)](https://www.therness.com/defects/601-arc-strike/)Miscellaneous imperfections — ISO 6520-1 group 6.

## Terms used on this page

[Heat input](https://www.therness.com/glossary/heat-input/)

Heat input is the energy delivered to a joint per unit length of weld, calculated from arc voltage, welding current and travel speed and multiplied by the thermal efficiency factor of the process.

[Hydrogen cracking](https://www.therness.com/glossary/hydrogen-cracking/)

Hydrogen cracking is a delayed fracture in or near a weld caused by diffusible hydrogen combining with a susceptible microstructure and tensile residual stress, typically appearing hours or days after welding is complete.

## Where this imperfection dominates

Structural steel fabrication and erection

### [Weld monitoring for structural steel fabrication](https://www.therness.com/applications/structural-steel/)

Shop-fabricated and site-erected steel under AWS D1.1 and EN 1090-2. The four monitoring pain points that cost structural fabricators most, and which Therness signal addresses each.

Offshore oil, gas and marine energy structures

### [Weld monitoring for offshore structures and pipelines](https://www.therness.com/applications/offshore/)

Fixed platforms, topside piping and subsea pipelines welded under classification-society rules and the transportation codes. The pain points that cost offshore fabricators most, and which Therness signal addresses each.

## Questions about radiating crack

### Is a radiating crack the same thing as a branching crack?

No. A branching crack is one crack that split as it grew; a radiating crack is several cracks sharing one point of origin, usually a hard zone left by an accidental arc strike.

### Does grinding out an arc strike remove the risk?

Only if the ground surface is then inspected. Grinding removes the visible mark, not necessarily the hardened zone beneath it, where a crack can still start later.

### Which forms first, the hard zone or the crack?

The hard zone. It forms the moment the accidental heating event quenches against cold metal, before any crack exists — which is why the fix targets the event, not the crack.

## See the condition, not the consequence

Most weld imperfections are produced by conditions that exist while the arc is running. Therness records those conditions on every weld, so a suspect run is known on the shift that made it rather than in a batch report.

[Book a technical call](https://www.therness.com/contact/) [See the thermal weld camera](https://www.therness.com/products/heatcam-ir-c/)