ISO 6520-1 group 1 · Cracks
ISO 6520-1 reference 105 is several separate cracks in the same region that share no common point of origin and do not connect. Cause matrix, the rule that tells the group apart from a single crack, and where acceptance is set.
A group of disconnected cracks is more than one crack in the same region of a joint, none touching, none traceable back to a single shared origin. That last condition separates ISO 6520-1 reference 105 from its two closest relatives: a radiating crack (103) is several cracks that share one point, and a branching crack (106) is one crack that split into connected paths. The rule is mechanical: trace each crack along its own length; if it reaches another crack or a shared point, it is not 105.
Because the underlying condition is usually distributed — hydrogen and restraint acting the same way at several points, or a material property varying unevenly through the plate — the cracks do not need a shared cause event, only a shared condition. That is also why the group is graded crack by crack: each is its own excluded finding, and repair removes and re-examines every one, not the one first found.
For inspection, the lesson is not to stop once the first crack in the region is confirmed. Interpass temperature drift across a long run is the condition most likely to produce several independent cold cracks, and a t8.5 cooling-time calculator check against the measured record is the fastest way to tell whether the whole length is suspect.
| Cause | Mechanism | Control |
|---|---|---|
| A hydrogen-cracking condition present along the whole joint | When hardenable microstructure, restraint and hydrogen are all present along a full run, cold cracks can start independently at several points. | Where preheat or interpass temperature drifted across a run, treat the whole length as suspect, not only the first crack found. |
| A parent material with unevenly distributed hardenability or cleanliness | Segregation bands or inclusions spread unevenly through the plate give several locations the same low local toughness at once. | Verify the cast and heat of the plate, not only the welding parameters, when the cause looks material rather than process. |
| Restraint distributed across a long, stiffened joint | A long, highly restrained joint can carry enough residual stress to exceed local capacity at more than one point. | Sequence and back-step long joints to spread residual stress instead of letting it build toward one end. |
The column that matters most is the last one. An inspection family marked as not finding this imperfection will not find it however carefully it is applied, and planning around that is cheaper than discovering it during a final examination.
| Family | Method | Capability | What it sees |
|---|---|---|---|
| Visual | Visual testing to ISO 17637 | Supporting signal | Finds each surface-breaking crack individually; the task is recording the whole group, not stopping at the first one. |
| Thermal | In-process infrared thermography | Supporting signal | A drifting interpass temperature or uneven cooling trend along the run points at the same distributed condition. |
| Camera | High-speed weld pool imaging | Limited | Most of these cracks form on cooling or after further passes, once the pool has already solidified. |
| NDT | Ultrasonic or phased array testing to ISO 17640 and ISO 13588, penetrant or magnetic particle testing for the surface trace | Primary route | Confirming several independent cracks, not one interconnected crack, changes repair scope and where reinspection looks. |
Therness pages never reproduce a standard's acceptance values: those tables are copyrighted and belong in the copy you hold. What follows is the pointer — which document governs, and which part of it to open.
| Standard | Clause topic | Note |
|---|---|---|
| ISO 5817 | Quality levels for imperfections indexed by ISO 6520-1 reference number; every crack in the group is excluded | No averaging: each crack in the group is its own excluded finding. |
| AWS D1.1 | Structural welding acceptance, treating any crack as a mandatory-repair finding regardless of count | Repair scope covers every crack in the group, not only the first one located. |
A radiating crack (103) is several cracks sharing one visible origin point. A group of disconnected cracks (105) has no shared point — each has its own independent origin.
No. They need the same underlying condition acting at more than one point — hydrogen and restraint present along the whole joint, for example — not one triggering event.
Several. Each crack in the group is its own excluded finding under a quality-level standard, and repair removes and re-examines every one, not only the first located.
Most weld imperfections are produced by conditions that exist while the arc is running. Therness records those conditions on every weld, so a suspect run is known on the shift that made it rather than in a batch report.