Discover HeatCore AI

ISO 6520-1 group 2 · Cavities

Elongated cavity (ISO 6520-1 ref. 2015): causes and detection

ISO 6520-1 reference 2015 is a non-tubular gas cavity stretched along the weld axis, distinct from a wormhole's tubular form. Cause matrix, the shape rule that tells the two apart, and where acceptance is set.

ISO 6520-1 reference
2015
Group
2 — Cavities
Also called
Elongated cavity, Elongated gas cavity, Elongated pore

An elongated cavity sits between an ordinary rounded pore and a wormhole: it is a non-tubular gas cavity stretched along the weld axis, lacking the tubular, roughly circular cross-section and the repeating herringbone array that identifies a wormhole on a radiograph. ISO 6520-1 reference 2015 exists because the distinction matters for both the read and the cause — a wormhole points at a sustained gas-generating condition, an elongated cavity more often at a brief interruption that recovered before it could tunnel.

The shape rule is the practical decision: a wormhole is tubular and frequently repeats in a herringbone array along the film; an elongated cavity is neither tubular nor patterned that way. That single visual distinction is what tells an inspector which designation, and which cause investigation, to write down.

The cause matrix follows the same logic as linear porosity — a row of separate pores, where an elongated cavity is one continuous one — and a brief gas-flow check against a heat input calculator run on the actual recorded current and travel speed usually tells whether the parameter window, rather than the shielding, is the likelier cause.

Typical causes

What produces elongated cavity, the mechanism, and the control that removes it
CauseMechanismControl
A brief loss of shielding gas coverageA short interruption — a draught, a worn nozzle, gun angle drifting — lets a gas pocket travel with the freezing front for a short distance before coverage recovers.Monitor gas flow continuously and treat a brief deviation as a candidate cause, not only a sustained one.
Localized contamination along a short section of the jointOil, moisture or scale confined to a short run releases gas only for that section, stretching the cavity without sustaining a full tunnel.Clean the full joint length; a short unclean section produces a proportionally short elongated cavity.
Pool turbulence from an unstable arc or excess currentA turbulent pool lets a bubble travel with the solidification front instead of floating out, in a shorter-lived version of what produces a wormhole.Measure current and arc stability per pass against the qualified window.

Detection: which route finds it

The column that matters most is the last one. An inspection family marked as not finding this imperfection will not find it however carefully it is applied, and planning around that is cheaper than discovering it during a final examination.

Detection routes for elongated cavity, and what each one can and cannot see
FamilyMethodCapabilityWhat it sees
VisualVisual testing to ISO 17637LimitedSubsurface unless it breaks through, and a surface break then reads as an ordinary pore, not as its elongated shape.
ThermalIn-process infrared thermographySupporting signalA gas-evolution anomaly of intermediate duration — longer than one pore, shorter than a sustained wormhole event — is the signature to flag.
CameraHigh-speed weld pool imagingSupporting signalA short burst of bubbling, distinct from an instantaneous spatter event or continuous bubbling, is the visual precursor.
NDTRadiographic testing to ISO 17636Primary routeShows an elongated trace with an irregular, non-tubular cross-section, unlike the tubular form and herringbone array that identify a wormhole; that shape difference is the whole basis for the two designations.

Where acceptance is defined

Therness pages never reproduce a standard's acceptance values: those tables are copyrighted and belong in the copy you hold. What follows is the pointer — which document governs, and which part of it to open.

Documents that set the acceptance criteria, and the clause topic to read
StandardClause topicNote
ISO 5817Quality levels for imperfections in steel, nickel and titanium joints, indexed by ISO 6520-1 reference numberAssessed on length like a wormhole is, but the two designations are not interchangeable. Read it in the standard.
API 1104Acceptance for pipeline girth welds, treated separately from structural workPipeline acceptance is its own regime; do not carry a structural criterion into it.

Questions about elongated cavity

How is an elongated cavity told apart from a wormhole on a radiograph?

By shape. A wormhole is tubular, with a roughly circular cross-section, and often repeats in a herringbone array; an elongated cavity is non-tubular and irregular, with no such array. That distinction, not the cause, is what gets reported.

Does an elongated cavity always mean sustained gas contamination?

No. That is the practical difference from a wormhole: an elongated cavity more often comes from a brief interruption that recovered before it could sustain a full tunnel.

Can both appear on the same weld?

Yes. Both come from a gas mechanism disturbing the same freezing pool — a short elongated cavity where a shielding loss was brief, a wormhole where it lasted longer.

See the condition, not the consequence

Most weld imperfections are produced by conditions that exist while the arc is running. Therness records those conditions on every weld, so a suspect run is known on the shift that made it rather than in a batch report.