Discover HeatCore AI

ISO 6520-1 group 3 · Solid inclusions

Flux inclusion (ISO 6520-1 ref. 302): causes and detection

ISO 6520-1 reference 302 is unfused flux carried into the weld metal, distinct from the fused slag of reference 301. Cause matrix, the test that tells them apart, and where acceptance is set.

ISO 6520-1 reference
302
Group
3 — Solid inclusions
Also called
Flux inclusion, Unfused flux

Reference 302 is what a flux inclusion becomes when the granular shielding material a flux-based process depends on never fully melts: instead of a continuous liquid slag layer that separates cleanly from the pool, a solid grain of unmelted flux is carried into the metal and frozen in place. It sits beside reference 301, slag inclusion, and the two are often confused on a radiograph, but 301 is fused material that failed to escape while 302 never melted in the first place.

The cause matrix in submerged arc welding is a flux-condition story: bed depth for the current in use, grain condition, and whether travel speed gives it time to melt before the pool freezes.

Detection splits by process: SAW’s flux blanket blocks any camera view of the pool at the time of welding, so radiography carries most of the burden there, while open-arc flux processes such as FCAW leave the pool visible to a camera throughout the run.

See reference 303, oxide inclusion, the other group-300 inclusion tied to a different shielding failure, and reference 3042, copper inclusion, the metallic member of the family.

Typical causes

What produces flux inclusion, the mechanism, and the control that removes it
CauseMechanismControl
Flux depth wrong for the current in SAWAn undersized bed vents gas and pulls in unmelted granules; an oversized one leaves cold flux at the edges the arc never reaches.Set flux depth from the qualified procedure for the current and wire diameter, not by habit.
Flux batch contaminated or wrong grain sizeRecycled fines or the wrong grain distribution melt unevenly, leaving unmelted particles instead of a continuous liquid slag.Screen recycled flux and store fresh flux to the supplier's condition limits.
Travel speed too high for the flux-current pairingA fast pool does not give flux enough dwell time to fully melt before solidification catches it.Measure travel speed against the qualified window, not bead appearance.

Detection: which route finds it

The column that matters most is the last one. An inspection family marked as not finding this imperfection will not find it however carefully it is applied, and planning around that is cheaper than discovering it during a final examination.

Detection routes for flux inclusion, and what each one can and cannot see
FamilyMethodCapabilityWhat it sees
VisualVisual testing to ISO 17637LimitedBuried under a SAW flux blanket during welding. A surface-breaking granule is visible on the finished pass on open-arc flux processes such as FCAW.
ThermalIn-process infrared thermographyLimitedUnmelted flux does not disturb the cooling curve the way a gas or slag event does.
CameraHigh-speed weld pool imagingLimitedNo camera view under a SAW flux blanket. FCAW is open-arc, so the pool is visible and unmelted flux is a catchable precursor.
NDTRadiographic testing to ISO 17636Primary routeUnmelted flux is less dense than the surrounding metal and gives clear film contrast, though it can resemble reference 301 on the same radiograph.

Where acceptance is defined

Therness pages never reproduce a standard's acceptance values: those tables are copyrighted and belong in the copy you hold. What follows is the pointer — which document governs, and which part of it to open.

Documents that set the acceptance criteria, and the clause topic to read
StandardClause topicNote
ISO 5817Quality levels for inclusions, indexed by ISO 6520-1 reference numberFlux inclusion is graded under the same inclusion rows as slag.
API 1104Acceptance for pipeline girth welds, assessed by radiographic interpretationPipeline acceptance is its own regime; do not carry a structural criterion into it.

Questions about flux inclusion

What is the difference between a flux inclusion and a slag inclusion?

Reference 301 is flux that melted and failed to float clear before the pool solidified. Reference 302 is flux that never melted at all and was carried in as a solid granule. A polished section under magnification shows 301 as a glassy, fused phase and 302 as a granular, unmelted particle.

Which welding process produces flux inclusions?

Submerged arc welding, because the flux bed is granular and unmelted grains sit at its edges throughout the run. Flux-cored arc welding can also produce it where the core flux fails to melt fully.

Can a pool camera catch a flux inclusion while welding?

Depends on the process. SAW runs under an opaque flux blanket with no camera view of the pool at all, so detection there depends on radiography after the run. FCAW is open-arc, so the pool is visible and unmelted flux is a catchable precursor.

See the condition, not the consequence

Most weld imperfections are produced by conditions that exist while the arc is running. Therness records those conditions on every weld, so a suspect run is known on the shift that made it rather than in a batch report.

Progetto cofinanziato nell'ambito del PR Piemonte FSE+ 2021-2027,
Priorità I, Obiettivo Specifico a), Azione 4 – "Sostegno alla nascita delle start up"