Discover HeatCore AI

ISO 6520-1 group 5 · Imperfect shape and dimension

Sagging (ISO 6520-1 ref. 509): causes and detection

ISO 6520-1 reference 509 covers sagging, a weld pool drooping under gravity into an asymmetric profile. Cause matrix, why the pool camera catches it before it freezes, and where acceptance is set.

ISO 6520-1 reference
509
Group
5 — Imperfect shape and dimension
Also called
Sagging, Drooping

Sagging is what a weld pool does when gravity has more influence over its shape than surface tension does: instead of staying centred on the joint, the pool flows toward the lower side before it freezes, leaving an asymmetric leg length rather than a fold at the toe. That distinguishes it from overlap, where filler folds over an already formed toe without fusing — sagging is the whole pool moving, not a flap of metal on top of it.

The imperfection is a gravity problem in every position. Horizontal and vertical joints see the pool slide sideways off centre; flat and overhead joints see it collapse toward the root instead — the same excess-fluidity condition that borders on burn-through. Pipeline girth welds see it often because a single joint is routinely welded through several positions in one pass.

Because the pool moves visibly while molten, the run gives a live signal rather than only a post-weld finding. A procedure verified per position, with deposition rate checked against a deposition rate calculator for the position in use, is the practical control before the first out-of-position pass runs.

Typical causes

What produces sagging, the mechanism, and the control that removes it
CauseMechanismControl
Heat input too high for the positionAn overly fluid, oversized pool cannot be held by surface tension against gravity: in horizontal or vertical work it slides sideways off centre, and in flat or overhead work it sags straight through the joint toward the root — the same excess-fluidity condition bordering on burn-through.Qualify current, voltage and travel speed specifically for the position, and treat a position change as its own parameter set.
Process or technique not adapted to an out-of-position jointA technique built for flat welding assumes the pool stays put; carried into a horizontal or vertical joint unchanged, it deposits more volume than gravity allows to stay in place.Qualify welders and procedures separately for each position rather than assuming a flat-position qualification covers it.
Weave or manipulation technique that does not counteract gravity's pull on the poolWithout a technique redirecting filler back toward the upper side of the joint, the pool's own weight biases it toward the lower side on every pass.Qualify and verify weave technique for the position in the cell, not only on a flat test coupon.

Detection: which route finds it

The column that matters most is the last one. An inspection family marked as not finding this imperfection will not find it however carefully it is applied, and planning around that is cheaper than discovering it during a final examination.

Detection routes for sagging, and what each one can and cannot see
FamilyMethodCapabilityWhat it sees
VisualVisual testing to ISO 17637, checking leg length or bead width symmetryPrimary routeThe asymmetric profile is externally visible and directly measurable once the weld has cooled.
ThermalIn-process infrared thermographySupporting signalA pool running hotter or larger than the qualified window shows an extended thermal signature before it visibly droops.
CameraHigh-speed weld pool imagingPrimary routeSagging is a visible flow event while it happens — the pool moving toward the lower side of the joint is the imperfection forming, not a precursor to it.
NDTVolumetric NDT (radiographic or ultrasonic testing)Does not find itSagging is external profile, not a subsurface condition; volumetric NDT says nothing about a pool having drooped while molten.

Where acceptance is defined

Therness pages never reproduce a standard's acceptance values: those tables are copyrighted and belong in the copy you hold. What follows is the pointer — which document governs, and which part of it to open.

Documents that set the acceptance criteria, and the clause topic to read
StandardClause topicNote
ISO 5817Quality levels for weld profile and position-related imperfectionsSet against the joint type and profile, not one figure for every position. Read it in the standard.
API 1104Acceptance for pipeline girth welds made in fixed, multi-position rotationA single girth weld routinely passes through every position, the condition sagging depends on.

Questions about sagging

Is sagging the same imperfection as overlap?

No, though gravity contributes to both. Overlap is filler folding over the toe without fusing; sagging is the whole pool shifting into an asymmetric profile.

Does sagging only occur in certain welding positions?

It is a gravity effect in every position: sideways off centre in horizontal work, or straight through the joint toward the root in flat and overhead work — both the same excess-fluidity condition that borders on burn-through.

Can sagging be caught before the weld finishes?

Yes. Because the pool visibly moves toward the lower side while molten, in-process pool imaging can flag the run before it solidifies into the finished profile.

See the condition, not the consequence

Most weld imperfections are produced by conditions that exist while the arc is running. Therness records those conditions on every weld, so a suspect run is known on the shift that made it rather than in a batch report.

Progetto cofinanziato nell'ambito del PR Piemonte FSE+ 2021-2027,