Discover HeatCore AI

ISO 6520-1 group 5 · Imperfect shape and dimension

Poor restart (ISO 6520-1 ref. 517): causes and detection

ISO 6520-1 reference 517 covers poor restart, a flaw at the point welding resumes after a stop. Cause matrix, why the location is known in advance, and the standards setting the acceptance limit.

ISO 6520-1 reference
517
Group
5 — Imperfect shape and dimension
Also called
Poor restart, Restart flaw, Recommencement flaw

Poor restart is a fusion or profile flaw at the point where welding resumes after a stop: an electrode change, a shift handover, or any interruption. The new arc must re-establish a stable pool on a crater the previous pass left cold and often concave, and without a deliberate technique the joint carries a small step, an underfill pocket or a local lack of fusion at that one location.

The finding concentrates causes that act independently elsewhere in the weld but arrive together at a restart: a cold arc strike, a crater carrying an unremoved shrinkage cavity, and parameters resuming at steady-state before the pool has re-stabilised. That is also why crater cracks and poor restart get discussed together so often — they share a location, not a mechanism: one is solidification shrinkage, the other an imperfect re-fusion.

Because the location is known in advance, it is one of the few imperfections a visual inspection can be told exactly where to look for. A high-speed weld pool camera watching that point shows directly whether the qualified restart technique — back-step, grind-out, ramped current — was actually followed.

Typical causes

What produces poor restart, the mechanism, and the control that removes it
CauseMechanismControl
Arc restruck without re-establishing a stable pool at the craterThe new arc starts on a cold, shallow crater, and the restart point fuses poorly or steps in profile before the pool re-stabilises.Qualify a restart technique — back-step, grind-out or ramped current — rather than restriking directly onto the crater.
Crater from the previous pass not prepared before restartingAn unground crater carries a shrinkage cavity or oxide film into the restart, so the new pass fuses over it instead of sound metal.Grind or dress the crater before every restart, planned or not.
Current or travel speed not ramped back to the qualified window at restartThe first moments of a restruck arc run cold or fast relative to the steady-state pass, reproducing a small fusion or underfill pocket at the transition.Qualify a restart ramp for current and travel speed rather than resuming at steady-state settings immediately.

Detection: which route finds it

The column that matters most is the last one. An inspection family marked as not finding this imperfection will not find it however carefully it is applied, and planning around that is cheaper than discovering it during a final examination.

Detection routes for poor restart, and what each one can and cannot see
FamilyMethodCapabilityWhat it sees
VisualVisual testing to ISO 17637, focused on every restart locationPrimary routeA step, local underfill or crater mark at a known restart point is directly visible once an inspector knows where to look.
ThermalIn-process infrared thermographySupporting signalThe restruck arc's first moments show a distinct thermal transient against the steady-state pass either side of it.
CameraHigh-speed weld pool imagingSupporting signalShows the pool re-establishing itself over the old crater, the clearest evidence of whether the restart technique was followed.
NDTUltrasonic or radiographic testing to ISO 17640 or ISO 17636LimitedUseful if a restart is suspected of hiding a lack-of-fusion pocket; otherwise visual inspection already answers it.

Where acceptance is defined

Therness pages never reproduce a standard's acceptance values: those tables are copyrighted and belong in the copy you hold. What follows is the pointer — which document governs, and which part of it to open.

Documents that set the acceptance criteria, and the clause topic to read
StandardClause topicNote
ISO 5817Quality levels for imperfect shape and dimension, indexed by ISO 6520-1 reference numberPoor restart is assessed as its own finding at the specific location, not folded into a general profile tolerance for the pass.
AWS D1.1Workmanship requirements for arc starts and stops on structural weldsStructural codes commonly require restart locations to be identifiable and inspected, independent of the general profile limit.

Questions about poor restart

Why do restarts need their own inspection attention?

A restart concentrates several problems in one small area — a cold arc start, an unprepared crater, a parameter ramp — so its defect rate runs higher than the weld either side of it.

Is poor restart the same imperfection as a crater crack?

No. A crater crack forms in the pool left at the end of a pass; poor restart is the fusion or profile flaw where the next pass begins over that crater. The two share a location, not a mechanism.

Does grinding out the crater before restarting actually help?

Yes. It removes the shrinkage cavity and any oxide film the crater carries, so the new arc starts on sound metal instead of fusing over a pre-existing flaw.

See the condition, not the consequence

Most weld imperfections are produced by conditions that exist while the arc is running. Therness records those conditions on every weld, so a suspect run is known on the shift that made it rather than in a batch report.