Discover HeatCore AI

Welding glossary

Defect sizing

Defect sizing is the measurement of an indication's dimensions once non-destructive testing has detected it — principally its length along the weld and its height or through-wall extent — and different NDT methods measure these two dimensions with very different accuracy.

Detecting a defect and sizing it are different jobs, and a method that excels at one can be mediocre at the other. Length — the extent of an indication measured along the weld — and height, meaning its through-wall or depth extent, are two different numbers, and a quality-level comparison, an ISO 6520-1 classification and a fitness-for-service calculation each depend on them to different degrees: length alone is often enough to classify an imperfection type, but height is what a fracture-mechanics assessment of a planar flaw actually needs.

Radiographic and direct visual methods read length reliably, because both project the joint onto a flat image or a direct view and a linear extent in that plane is a straightforward measurement. Height is the dimension they struggle with: film density and geometric assumptions stand in for a direct through-wall reading, and the result degrades for a flaw that is not favorably oriented to the beam — the reason a planar defect like lack of fusion is harder to size by radiography than a rounded one like gas pore. Ultrasonic techniques split on the same axis, but not as one method. Phased-array (ISO 13588) and time-of-flight diffraction (ISO 10863) size through-wall height from diffracted sound travel time at the flaw tip — a physical measurement rather than an inference. Conventional pulse-echo UT under ISO 17640 sizes height a different way, by amplitude drop against a reference reflector, and that inference carries materially wider uncertainty than a diffraction-based reading. All three still build length the same way, by scanning and stitching multiple probe positions, which is comparatively coarser than their height reading. Surface methods — magnetic particle and liquid penetrant testing — size length at the surface only and give no through-wall information at all, because neither can see below the surface it is applied to.

Choosing an NDT method for a joint is therefore partly a sizing decision, not only a detection one: the acceptance criterion that actually governs the joint decides which dimension has to be trusted, and that decides which method belongs on the joint.

Where you meet this term

  • Fitness-for-service and engineering critical assessments, where flaw height feeds a fracture-mechanics calculation and length alone is not enough
  • Acceptance decisions at a quality-level boundary, where a marginal indication is re-measured by a second method before disposition
  • Radiographic and ultrasonic inspection reports, where length and through-wall extent are recorded as two separate values, not one
  • NDT method selection for a joint, made partly on which dimension the governing acceptance criterion actually depends on