# Dilution

Source: https://www.therness.com/glossary/dilution/
Language: en

Welding glossary

Dilution is the proportion of deposited weld metal that originates from melted base metal rather than from the filler, expressed as a fraction of the total deposit.

Unit

%

Formula

D = A\_base / (A\_base + A\_filler), the melted parent-metal area over the total fused area

[Weld dilution calculator](https://www.therness.com/tools/weld-dilution-calculator/)

Full guide

[Dilution: the long-form guide](https://www.therness.com/blog/weld-overlay-cladding-quality-monitoring-thermal-imaging/)

This page defines the term. The guide works through how it is calculated, controlled and evidenced.

Every weld pool mixes two sources of metal: the filler being added and the base metal the arc melts as it advances. Dilution is the share that comes from the base metal. For a structural butt or fillet weld this is rarely discussed, because filler and base metal are usually similar alloys and the mix barely changes the outcome. For overlay and cladding welding it is the central variable, because the entire point of the deposit is to put a different alloy — a corrosion-resistant or wear-resistant layer — on top of a cheaper structural base metal, and dilution is what determines how much of that base metal ends up inside the layer meant to protect it.

Higher dilution pulls the deposit’s chemistry toward the base metal and away from the filler’s intended composition. On a corrosion-resistant overlay this can move the alloy below the composition its corrosion performance depends on; on a hardfacing deposit it can soften the working surface. Both failures are invisible on the surface and only show up in service or on a chemical analysis of the deposit — a much later and more expensive point to discover them.

Dilution is controlled through the same variables that shape [penetration](https://www.therness.com/glossary/penetration/): heat input, travel speed, and the process itself. Single-pass, high-energy processes drive molten base metal deep into the [weld pool](https://www.therness.com/glossary/weld-pool/) and dilute heavily; multi-layer strip cladding, where later layers barely touch the original base metal, dilutes far less. Because the mechanism is the same energy-and-travel-speed relationship that governs penetration, real-time thermal monitoring of an overlay pass reads as a consistency check on dilution even though it cannot measure deposit chemistry directly: a heat input excursion on an overlay pass is a dilution excursion by the same physics that makes it a penetration excursion on a structural weld.

## Where you meet this term

- Corrosion-resistant overlay and cladding welding, where the specification exists specifically to control it
- Dissimilar-metal joints, where filler chemistry is chosen assuming a known dilution level
- Hardfacing deposition, where excess dilution softens the wear-resistant layer being built up
- Procedure qualification for overlay welds, where deposit chemistry is verified against the assumed dilution by analysis

## Related terms

[Weld pool](https://www.therness.com/glossary/weld-pool/)

The weld pool is the localized volume of molten metal created by the welding heat source, into which filler metal is added and from which the weld bead forms as it solidifies.

[Penetration](https://www.therness.com/glossary/penetration/)

Penetration is the depth to which weld metal and the fusion boundary extend into the parent material, measured from the original joint surface inward.

## Applications where it is controlled

Pressure equipment and process plant

### [Weld monitoring for pressure vessels](https://www.therness.com/applications/pressure-vessels/)

Thick-section, multi-pass, code-governed welding. The codes that apply, the four monitoring pain points that cost pressure-vessel fabricators most, and which Therness signal addresses each.

[All glossary terms](https://www.therness.com/glossary/)