A dissimilar metal weld (DMW) joins two base metals of different chemical composition or metallurgical family — most commonly a ferritic or low-alloy steel to an austenitic stainless or nickel-base alloy — so the fusion zone sits between two materials with different thermal, mechanical and microstructural behaviour rather than one.

A dissimilar metal weld exists the moment the two sides of the joint stop being the same material family: a low-alloy ferritic steel welded to an austenitic stainless pipe, or a nickel-base alloy welded to carbon steel, are the joints the name describes. Everything the dilution ratio and the filler-metal choice manage in a similar-metal weld — a fusion zone whose chemistry sits close to the base metal on both sides — no longer holds, because the fusion zone’s chemistry now depends on how much of two different base metals melted into it, and by how much.

Three failure mechanisms are specific to this joint type and do not appear, or appear far more weakly, in a similar-metal weld.

Fusion-line martensite from dilution. When the ferritic side dilutes an austenitic filler more than the filler composition was chosen to absorb, the actual weld-metal chemistry at the fusion line can shift into a martensite-forming region the filler was selected to avoid. The resulting martensite band sits precisely at the fusion line — the narrowest, most highly stressed part of the joint — which is exactly where hydrogen cracking initiates when it occurs.

Carbon migration under prolonged elevated-temperature service. Carbon diffuses from higher chemical activity toward lower activity, and the strong carbide-forming elements in an austenitic filler give the weld-metal side lower carbon activity than a ferritic base metal at service temperature. Over months or years of elevated-temperature exposure, carbon migrates out of the ferritic heat-affected zone toward the fusion line, leaving a soft, carbon-depleted band on the ferritic side — a slow, one-directional degradation a similar-metal joint does not experience.

Thermal-expansion mismatch. Austenitic alloys expand and contract noticeably more per degree than ferritic steels. Every thermal cycle the joint sees in service imposes a differential strain concentrated at the fusion line, on top of whatever residual stress the weld already carries from cooling — a fatigue driver a similar-metal joint, where both sides expand together, does not have. A nickel-base filler is the standard choice for this joint precisely because its coefficient of thermal expansion and its carbon activity both sit between the ferritic and austenitic sides, which narrows — without eliminating — both mechanisms above.

None of the three is prevented by getting heat input or carbon equivalent right on a single-alloy basis; each has to be assessed for the specific pair of base metals and the filler chosen to sit between them.

Where you meet this term

  • Boiler and heat-recovery steam generator tube-to-header transition welds between ferritic and austenitic alloys
  • Pipeline tie-ins joining different steel grades or wall chemistries
  • Filler-metal selection for a joint where the two base metals sit in different ISO/TR 15608 groups
  • Failure investigations of a crack sitting exactly at the fusion line rather than in either base metal