# Heat input

Source: https://www.therness.com/glossary/heat-input/
Language: en

Welding glossary

Heat input is the energy delivered to a joint per unit length of weld, calculated from arc voltage, welding current and travel speed and multiplied by the thermal efficiency factor of the process.

Symbol

Q

Unit

kJ/mm (EN and ISO practice); J/in (ASME and AWS practice)

Formula

Q = k × (U × I × 60) / (v × 1000), with U in volts, I in amperes and v in mm/min

[Heat input calculator](https://www.therness.com/tools/heat-input-calculator/)

Full guide

[Heat input: the long-form guide](https://www.therness.com/blog/welding-heat-input-calculation-quality-control/)

This page defines the term. The guide works through how it is calculated, controlled and evidenced.

Heat input is the quantity that connects the settings on a power source to the metallurgy of the finished joint. It fixes how fast the weld and the surrounding parent material cool, and cooling rate is what decides hardness, toughness and the structure of the heat-affected zone.

Two conventions share the name, and confusing them is the most common error in practice. **Arc energy** is the electrical energy per unit length, straight out of the formula. **Heat input** in the EN and ISO sense is that value multiplied by a thermal efficiency factor *k* that accounts for the share of the arc energy actually entering the joint — different for submerged arc, for the consumable-electrode gas-shielded processes, and for tungsten arc welding. ASME and AWS documents use the unfactored value and call it heat input. Two records can therefore quote heat input for the same weld and differ substantially, so the convention belongs next to the number.

The travel speed term carries most of the measurement error. Voltage and current are read off the power source; speed is usually estimated, and because heat input varies inversely with it, a speed that is wrong by a fifth moves the result by more than the width of many qualified bands. Weave makes this worse and invisible at the same time: a wider weave means slower advance along the joint at identical meter readings.

Where a procedure qualification carries impact or hardness testing, the qualified value is bounded on one side or both. A production weld outside those bounds is outside the qualification, whatever the finished bead looks like — which is the practical reason to compute it from measured values rather than from the figures on the sheet.

## Where you meet this term

- Welding procedure specifications and qualification records, where it is a controlled variable
- Cooling rate and microstructure assessment in the heat-affected zone
- Hardness and toughness arguments during a procedure qualification review
- Distortion and residual stress prediction for thin or restrained sections

## Related terms

[Interpass temperature](https://www.therness.com/glossary/interpass-temperature/)

Interpass temperature is the temperature of the weld metal and adjacent parent material in a multi-run weld immediately before the next run is started.

## Standards that use this term

- [ASME BPVC Section IX](https://www.therness.com/standards/asme-ix/)ASME Section IX (BPVC Section 9) qualifies welding procedures (WPS, PQR) and welders (WPQ). When it applies, the codes that invoke it, and the records that prove it.

## Imperfections this term relates to

- [Incomplete fusion (ref. 401)](https://www.therness.com/defects/401-lack-of-fusion/)Lack of fusion and penetration — ISO 6520-1 group 4.

[All glossary terms](https://www.therness.com/glossary/)