# Linear indication

Source: https://www.therness.com/glossary/linear-indication/
Language: en

Welding glossary

A linear indication is an indication whose length is greater than three times its width, as ISO 23278 defines it for magnetic particle testing of ferromagnetic steel welds; an indication whose length is less than or equal to three times its width is non-linear.

Full guide

[Linear indication: the long-form guide](https://www.therness.com/blog/magnetic-particle-testing-welds-procedure-standards-acceptance-criteria/)

This page defines the term. The guide works through how it is calculated, controlled and evidenced.

A linear indication is a shape class, not the name of a flaw. ISO 23278:2015, the acceptance-level standard for magnetic particle testing of ferromagnetic steel welds, defines it as an indication whose length is greater than three times its width. Everything else is a non-linear indication: its length is less than or equal to three times its width. The boundary case is easy to miss. An indication exactly three times as long as it is wide is non-linear.

The class matters because the standard sets a separate limit for each class at every acceptance level. A linear indication is assessed on its length, a non-linear one on its major-axis dimension. Those values belong to the standard, so look them up in the edition your contract names. The test method itself sits in [ISO 17638](https://www.therness.com/standards/iso-17638/). The class is read from the length and width of the trace alone, so it cannot say what produced the trace. Classing and assessing both use the length measured on the surface; magnetic particle testing does not measure through-wall height, which is covered under [defect sizing](https://www.therness.com/glossary/defect-sizing-ndt/).

## Worked example: line or dot?

Magnetic particle testing of a ferritic steel weld toe leaves three traces. Their sizes are in arbitrary units, so nothing here reads as a limit: A is 5 long and 1 wide, B is 3 long and 1 wide, and C is 2 long and 1 wide.

- A is five times as long as wide, which is more than three, so it is **linear**.
- B is exactly three times as long as wide. That is not more than three, so it is **non-linear**, even though it looks like a short line.
- C is twice as long as wide, so it is **non-linear** as well.

B and C land in the same class and are assessed the same way. Now suppose A and B sit on one line with a gap of 2 units. That gap is less than the major dimension of the smaller trace, B, which is 3 units, so ISO 23278 has them assessed as a single continuous indication. Measured end to end, gap included, it is 10 units long and 1 wide, which makes it linear: not a long trace and a short one.

None of this is a verdict. The class selects which row of the acceptance table applies. At level 2X or 3X, every linear indication detected is assessed to level 1, although indications smaller than the original level may not be detected reliably. The [acceptance criteria](https://www.therness.com/glossary/acceptance-criteria-welding/) your contract names decide what happens next. A surface method that reports an instrument signal instead of a visible trace is a different case: see [eddy current testing](https://www.therness.com/glossary/eddy-current-testing-ect/).

## Where you meet this term

- Magnetic particle examination reports, where indications that reach the evaluation level are classed by length and width and assessed against the acceptance level the contract names
- Acceptance-level tables that give linear and non-linear indications separate limits
- Adjacent-indication assessment, where indications closer together than the major dimension of the smaller one are assessed as a single continuous indication
- Surface NDT interpretation, where a trace is read before anyone calls it an imperfection

## Related terms

[Defect sizing](https://www.therness.com/glossary/defect-sizing-ndt/)

Defect sizing is the measurement of an indication's dimensions once non-destructive testing has detected it — principally its length along the weld and its height or through-wall extent — and different NDT methods measure these two dimensions with very different accuracy.

[Acceptance criteria (welds)](https://www.therness.com/glossary/acceptance-criteria-welding/)

Acceptance criteria for a weld are the combined rule set that decides pass or fail: which quality level of imperfection applies, which acceptance level a specific inspection method invokes, and what extent of inspection is required before the two can be checked at all.

## Standards that use this term

- [ISO 17638](https://www.therness.com/standards/iso-17638/)Does ISO 17638 apply to your weld? Scope decision flow for the magnetic particle testing standard, the materials it excludes, and the records that support an MT inspection report.
- [ISO 17635](https://www.therness.com/standards/iso-17635/)Does ISO 17635 tell you which NDT method to use, or just how to frame the decision? Scope decision flow for the general-rules standard for non-destructive testing of welds, and the method standards it sits above.

## Imperfections this term relates to

- [Longitudinal crack (ref. 101)](https://www.therness.com/defects/101-longitudinal-crack/)Cracks — ISO 6520-1 group 1.
- [Surface pore (ref. 2017)](https://www.therness.com/defects/2017-surface-pore/)Cavities — ISO 6520-1 group 2.

[All glossary terms](https://www.therness.com/glossary/)