Welding glossary

Travel speed range (WPS)

A travel speed range in a welding procedure specification is the lowest and highest travel speed the WPS permits for a weld pass, a band written on the document rather than a value measured on any one weld.

Unit
mm/min (in/min in ASME and AWS practice)
Formula
Arc energy at a given speed: E = (60 × U × I) / (1000 × v) in kJ/mm, with U in volts, I in amperes and v in mm/min

A travel speed range is a document value: two numbers, a lower and an upper bound, that a welding procedure specification (WPS) allows for a weld pass. It is not a measurement. ASME Section IX’s suggested WPS format, Form QW-482, shows where it lives. Its electrical characteristics table has a “Travel Speed (Range)” column, filled in per weld-pass row, beside Amps (Range), Volts (Range) and Wire Feed Speed (Range), and a separate “Heat Input (max.)” line sits under the table. The form is a suggested layout. Under the ISO scheme, ISO 15609-1 sets what an arc-welding WPS must contain.

Three different numbers get called travel speed, and only one of them is the range. The programmed value is what the program or the welder aims for. The measured value is what the arc actually did on a given weld, the quantity described under travel speed. The range is the permitted band. A compliance check compares the measured value with the range, and a programmed value inside the range does not by itself show that the weld stayed inside it.

Worked example: programmed, measured, permitted

A WPS pass permits 250 to 350 mm/min, 200 to 240 A and 23 to 26 V (illustrative values), and the weld runs at 24 V and 220 A. The robot program says 300 mm/min, which is inside the band. Suppose the program speed is set along the weave path: on the weld, the net advance along the joint measures 240 mm/min.

  • At the programmed 300 mm/min, arc energy is 60 × 24 × 220 ÷ (1000 × 300) = 1.056 kJ/mm.
  • At the measured 240 mm/min it is 60 × 24 × 220 ÷ (1000 × 240) = 1.32 kJ/mm, a quarter more.

The programmed value is inside the range and the measured one is below the lower bound, so the weld is outside what the WPS permits, whatever the program says. The same arithmetic shows how wide the energy band gets when the ranges combine freely. With those ranges, the permitted arc energy runs from about 0.79 to about 1.50 kJ/mm. A procedure that has to control energy therefore states a maximum heat input, and QW-482 has a separate “Heat Input (max.)” line for it. Check the convention before comparing with that line: ASME and AWS documents call the unfactored value heat input, while EN and ISO heat input applies a process efficiency factor. See heat input.

Whether the WPS band can be widened by revision or needs a new qualification is decided by the governing code’s variable tables, not by this page; a weld made outside the band is outside the WPS either way. See essential variable.

Where you meet this term

  • The electrical-characteristics table of ASME's suggested WPS form, where a speed range is written per weld-pass row beside the current, voltage and wire feed ranges
  • Production compliance checks, where a measured pass speed is compared with the band rather than with the programmed value
  • Heat input reviews, where the lower speed bound is the end of the range that delivers the most energy
  • Robotic and mechanised program set-up, where the programmed speed is chosen to sit inside the permitted band